Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 45.0 kg
99.2 lb (mass)
Load Weld Index
ChevronTexaco ISO 150 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..
Four Ball Extreme Pressure, Weld Load 45.0 kg
99.2 lb (mass)
Load Weld Index
ChevronTexaco ISO 68 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..