Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® LC200 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® LC80 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 1 Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
ConocoPhillips Tacna® Rx NLGI No. 1 Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
Dow Corning MOLYKOTE® 3451 CHEMICAL RESISTANT BEARING GREASE Fluorosilicone grease thickened with PTFEInformation provided by Dow Corning |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
Dow Corning MOLYKOTE® 3452 CHEMICAL RESISTANT VALVE GREASE Fluorosilicone grease thickened with PTFEInformation provided by Dow Corning |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
Dow Corning MOLYKOTE® G-0103 GREASE Mineral base multi-service grease designed for extended lubrication of bearingsInformation provided by Dow Corning |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | ASTM D2596, DIN 51 350 |
Chesterton 787 Sliding Paste Description: Chesterton® 787 Sliding Paste is a premium quality pure synthetic lubricant that will function affectivity even at ultra high temperatures and pressures. Designed for the most severe o.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | ASTM D2596, DIN 51 350 |
Chesterton 785 Parting Lubricant Description: Chesterton® 785 Parting Lubricant represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants in a non-carbonizing, ashless sy.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | Weld Point |
ChevronTexaco Delo® NLGI 0 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | Weld Point |
ChevronTexaco Delo® NLGI 00 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
ConocoPhillips 1 Milube® Grease 2100 NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | 1770 rpm, 80°F (27°C); ASTM D-2596 |
ConocoPhillips EP Polyurea NLGI Grade No. 1 Polyurea Greases offer significant performance advantages in high temperature, multipurpose, long-life and wet applications over conventional soap thickened greases. The nonsoap, polyurea thickener,.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | ASTM D 2596 |
ConocoPhillips Gear Shield NC Open Gear Lubricant Description: Conoco Gear Shield NC is a black, viscous fluid designed to lubricate open gears. Gear Shield NC contains neither chlorinated solvents nor lead compounds. Gear Shield NC is designed to .. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | Weld Point |
ChevronTexaco Black Pearl® NLGI 1 Grease EP FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | Weld Point |
ChevronTexaco Black Pearl® NLGI 2 Grease EP FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
ChevronTexaco Coupling Grease NLGI Grade 0/1 Texaco Coupling Grease delivers value through:Superior film strength — Formulated with a high viscosity base oil and polymer for superior film strengthLittle to no oil separation in high-speed coup.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | ASTM D-2596 |
ConocoPhillips 595 NC Open Gear Lube Description: Conoco Open Gear Lube 595 NC is a black, viscous, semi-fluid product that can be applied via central pumping systems that utilize injectors and nozzles for spray or drip application. Op.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | 1770 rpm, 80°F (27°C); ASTM D-2596 |
ConocoPhillips EP Polyurea NLGI Grade No. 2 Polyurea Greases offer significant performance advantages in high temperature, multipurpose, long-life and wet applications over conventional soap thickened greases. The nonsoap, polyurea thickener,.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | ASTM D2596 |
ConocoPhillips Grade 1 Calcium M Grease NLGI Description: Conoco Calcium M Grease is a specialty product that incorporates high load-carrying and antiwear capabilities with excellent low temperature properties and high-temperature stability af.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | |
ConocoPhillips Tacna® Rx NLGI No. 2 Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor.. |
|||
Four Ball Extreme Pressure, Weld Load | 400 kg | 882 lb (mass) | Weld Point |
ChevronTexaco Ulti-Plex® NLGI 1 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |