Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 163.1 kg | 359.6 lb (mass) | |
Dow Corning MOLYKOTE® 7325 GREASE Silicone grease especially for overrunning clutches in starter motorsInformation provided by Dow Corning |
|||
Four Ball Extreme Pressure, Weld Load | 163.1 kg | 359.6 lb (mass) | |
Dow Corning MOLYKOTE® PG-21 PLASTISLIP GREASE Silicone grease especially for plastic/plastic and plastic/metal combinations like control cables and circuit lever systemInformation provided by Dow Corning |