Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.00 - 21.0 kJ/m² @Temperature -40.0 - -30.0 °C |
1.43 - 9.99 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 7.14 kJ/m² Grade Count:22 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |