Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.30 - 19.0 kJ/m² | 0.619 - 9.04 ft-lb/in² | Average value: 3.13 kJ/m² Grade Count:23 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched (ISO) | 12.0 - 19.0 kJ/m² @Temperature -30.0 - -30.0 °C |
5.71 - 9.04 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 15.5 kJ/m² Grade Count:2 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 19.0 kJ/m² @Temperature -40.0 - -20.0 °C |
2.38 - 9.04 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 10.2 kJ/m² Grade Count:111 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Notched (ISO) | 6.00 - 19.0 kJ/m² @Temperature -40.0 - -20.0 °C |
2.86 - 9.04 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 11.6 kJ/m² Grade Count:11 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |