Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.50 - 14.0 kJ/m² | 4.04 - 6.66 ft-lb/in² | Average value: 11.9 kJ/m² Grade Count:4 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 14.0 kJ/m² @Temperature -40.0 - -30.0 °C |
0.952 - 6.66 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 5.75 kJ/m² Grade Count:5 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 14.0 kJ/m² @Temperature -40.0 - -30.0 °C |
0.952 - 6.66 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 6.80 kJ/m² Grade Count:4 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 3.00 - 14.0 kJ/m² | 1.43 - 6.66 ft-lb/in² | Average value: 7.41 kJ/m² Grade Count:39 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched (ISO) | 3.00 - 14.0 kJ/m² @Temperature -30.0 - -30.0 °C |
1.43 - 6.66 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.45 kJ/m² Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 14.0 kJ/m² @Temperature -30.0 - -30.0 °C |
5.71 - 6.66 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 13.0 kJ/m² Grade Count:4 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 14.0 kJ/m² @Thickness 3.20 - 3.20 mm |
5.71 - 6.66 ft-lb/in² @Thickness 0.126 - 0.126 in |
Average value: 13.0 kJ/m² Grade Count:4 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 14.0 kJ/m² @Temperature -30.0 - -30.0 °C |
5.71 - 6.66 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 12.6 kJ/m² Grade Count:6 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 14.0 kJ/m² @Thickness 3.20 - 3.20 mm |
5.71 - 6.66 ft-lb/in² @Thickness 0.126 - 0.126 in |
Average value: 12.6 kJ/m² Grade Count:6 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched (ISO) | 1.90 - 14.0 kJ/m² @Temperature -40.0 - -30.0 °C |
0.904 - 6.66 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 5.84 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Izod Impact, Notched (ISO) | 14.0 - 14.0 kJ/m² @Temperature -30.0 - -30.0 °C |
6.66 - 6.66 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 14.0 kJ/m² Grade Count:1 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 3.40 - 14.0 kJ/m² | 1.62 - 6.66 ft-lb/in² | Average value: 6.40 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |