Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.00 - 42.0 kJ/m² | 3.81 - 20.0 ft-lb/in² | Average value: 26.4 kJ/m² Grade Count:16 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 5.00 - 42.0 kJ/m² | 2.38 - 20.0 ft-lb/in² | Average value: 12.6 kJ/m² Grade Count:28 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 42.0 kJ/m² @Temperature -40.0 - -30.0 °C |
0.952 - 20.0 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 10.8 kJ/m² Grade Count:8 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |