Polymer Property : Izod Impact, Notched (ISO) = 9.66 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 20.3 kJ/m²
9.66 ft-lb/in²
ISO 180-93
Wellman Wellamid® GF1750-N1 50% Glass Fiber Reinforced Nylon 6
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.