Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 19.6 kJ/m² | 9.33 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, UV stabilized and characterized by a high fluidity of the melt, for injection molding.Available in: Europe and North America Pr.. |
|||
Izod Impact, Notched (ISO) | >= 19.6 kJ/m² | >= 9.33 ft-lb/in² | |
Sibur ABS 1106 Extrusion Grade ABS Plastic With high deformation properties and sanitary-hygienic properties for production of sheets with following pneumatic and vacuum forming of internal parts of refrigerators, as well as for compounding .. |
|||
Izod Impact, Notched (ISO) | >= 19.6 kJ/m² | >= 9.33 ft-lb/in² | |
Sibur ABS 1106M Extrusion Grade ABS Plastic With high thermal and light resistance for production of sheets with following pneumatic and vacuum formation of internal parts for refrigerators and other articles of technical purpose. |
|||
Izod Impact, Notched (ISO) | >= 19.6 kJ/m² | >= 9.33 ft-lb/in² | |
Sibur ABS 1530 Molding Grade ABS Plastic Thermal resistance with higher fluidity for large and thin wall articles. |