Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 17.2 kJ/m² | 8.18 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |