Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 10.5 kJ/m² @Temperature 23.0 °C |
5.00 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² @Temperature 23.0 °C |
5.00 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² | 5.00 ft-lb/in² | ISO 180/A |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² @Temperature 23.0 °C |
5.00 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² | 5.00 ft-lb/in² | ISO 180 |
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² | 5.00 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF1497-BK 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66 Description: Glass Fiber Reinforced, Silicone Lubricated Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² | 5.00 ft-lb/in² | ISO 180 |
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 40% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² | 5.00 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene J 690 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² @Temperature -20.0 °C |
5.00 ft-lb/in² @Temperature -4.00 °F |
ASTM D256 |
C.O.I.M. LARIPUR® LPR5760 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Izod Impact, Notched (ISO) | 10.5 kJ/m² | 5.00 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl A2H V25 Flame Retardant Nylon 66, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast. |