Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.10 kJ/m² | 4.33 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Izod Impact, Notched (ISO) | 9.10 kJ/m² | 4.33 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF1398 BK12 30% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 9.10 kJ/m² | 4.33 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |