Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.40 kJ/m² @Temperature 22.8 °C |
4.00 ft-lb/in² @Temperature 73.0 °F |
ISO 180/1A |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Izod Impact, Notched (ISO) | 8.40 kJ/m² | 4.00 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
Izod Impact, Notched (ISO) | 8.40 kJ/m² | 4.00 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
Izod Impact, Notched (ISO) | 8.40 kJ/m² | 4.00 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Izod Impact, Notched (ISO) | 8.40 kJ/m² | 4.00 ft-lb/in² | ISO 180/1A |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)
(Unverified Data**) Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad.. |