Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 121R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 121R PC (Europe-Africa-Middle East) LEXAN 121R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 121R is available in transparent, translucent and opaque colours. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 915AU PC LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 915R PC (Europe-Africa-Middle East) Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties... |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD121R PC (Europe-Africa-Middle East) LEXAN FXD121R is a transparent/translucent low viscosity grade for light diffusion special effects. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LI1813R PC (Europe-Africa-Middle East) Low-viscosity multi-purpose PC having low levels of ionics species. UV-stabilized. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LI1911R PC (Europe-Africa-Middle East) Low-viscosity multi-purpose grade having low levels of ionics species. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX2110T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2110T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX2114 PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific) 10 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML3042 PC (Europe-Africa-Middle East) LEXAN ML3042 offers an extremely low light transparency in combination with a very high reflection. This product is ideally suited for lighting reflectors. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
63.5*12.7*3.2; ISO 180/4A |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2800 PC (Europe-Africa-Middle East) PC2800 resin is a high flow (MFR = 28 at 300°C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release... |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific) LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Thickness >=5.00 mm |
30.9 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | DAM; Partial; ISO 180/1A |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient.. |
|||
Izod Impact, Notched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |