Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Asia Pacific) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 246 M PA6, DRY Description: Unreinforced polyamide 6, with high impact resistance, for injection molding. Grade formerly known as PSB196.Available in: EuropeProduct Applications: It is particularly adapted to the .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 0.000 °C |
26.2 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 0.000 °C |
26.2 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East) PBT+PC blend for painted automotive exterior applications, having good flow. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Thickness >=5.00 mm |
26.2 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML3485 PC (Europe-Africa-Middle East) LEXAN ML3485 is a low viscosity grade exhibiting an improved ductility over standard polycarbonate grades at equal flow. |