Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 0.000 °C |
20.0 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 0.000 °C |
20.0 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180/A |
Iran Petrochemical (PCC) 1922T Low Density Polyethylene LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Co.. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180/1A |
Styron INSPIREâ„¢ TF0808S(U) Polypropylene TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE .. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF RN001IX4 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RN001X4 is a compound based on PA 66 resin containing MoS2. Added features include: Internally Lubricated, High Impact, Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 LNP* VERTON* RV00AE is a compound based on Nylon 66 containing 50% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180/1A |
ExxonMobil LLDPE LL 6201RQ Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go.. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | ISO 180/1A |
ExxonMobil LLDPE LL 6201XR Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go.. |