Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Mytex Polymers AS33L-16 Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33L-16 is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and goo.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS PC+ ABS Automotive applications |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DI001E PC (Europe-Africa-Middle East) LNP* Lubricomp* DI001E is a compound based on Polycarbonate resin containing Silicone. Added features include: Internally Lubricated, Easy Molding. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND HI 10 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents. Main application fields: autom.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® MX 1000 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® MX 1001 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 0.000 °C |
19.0 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Borealis Borcoat™ BA213E Polypropylene for Steel Pipe Coating Borcoat™ BA213E is a polypropylene compound used as a component in thermal insulation coating systems. Applications: Borcoat™ BA213E is recommended as a polymer to make foam for thermal insulatio.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® XT1627-GY1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180 |
Polyram PlusTek PB841 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Izod Impact, Notched (ISO) | 39.9 kJ/m² | 19.0 ft-lb/in² | ISO 180/A |
ExxonMobil Exxtral™ BMV 201 Performance Polyolefin Product Description: A specialty thermoplastic olefin injection molding compound resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for large automotive e.. |
|||
Izod Impact, Notched (ISO) | 39.9 kJ/m² | 19.0 ft-lb/in² | ISO 180/A |
ExxonMobil Exxtral™ H1725 Performance Polyolefin Product Description: A specialty thermoplastic olefin compound resin with good flow, cold temperature resistance, high flexural modulus, low CLTE, and excellent paintability for automotive exterior .. |
|||
Izod Impact, Notched (ISO) | 39.9 kJ/m² | 19.0 ft-lb/in² | ISO 180/1A |
ExxonMobil LLDPE LL 6301XR Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO Test |
BASF Ultramid® B29 HM 01 PA6 (Dry) Ultramid B29 HM 01 is a medium viscosity , heat stabilized, PA6 universal wire jacketing resin offering excellent performance through the range of THHN, THWN, and TFFN constructions. It possesses a.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Polyplastic Armlen® PP 3IM Impact Modified Polypropylene Impact modified polypropylene composite materialInformation provided by PolyPlastic Group. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton UX06451 PPA LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |