Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CB285 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB285 high melt flow, 1,300 MPa flexural modulus, low CLTE, UV-stabilized, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of .. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer (Europe-Africa-Middle East) Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | ISO Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Europe-Africa-Middle East) High modulus/impact/heat PPE+PP. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL WCV072 PPE+PP Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² @Temperature -40.0 °C |
17.1 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON WV006 PBT (Europe-Africa-Middle East) LNP VERTON* WV006 is a compound based on Polybutylene Terephalate resin containing Long Glass. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | ISO 179 |
Bulk Molding Compounds BMC 665 Mineral filled, 20% glass reinforced polyester molding compound Description: BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good.. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | ISO 179 |
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o.. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® MD-TPE MD TPE - Impact Modified Polypropylene Copolymer Compound for Automobile Bumpers High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermotuf P1000IX3 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* P1000IX3 is a compound based on PA6 resin containing Impact Modifier. Added features include : High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural. |