Polymer Property : Izod Impact, Notched (ISO) = 14.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® C7410 PC+ABS (Asia Pacific)
Cycoloy* C7410 resin is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
ISO 180
Phillips Sumika Marlex® CHP-370 Thermoplastic Polyolefin  (discontinued **)
Thermoplastic Polyolefin, Good Stiffness and Impact PerformanceApplications: Automotive Pillar TrimConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.8-1.0%Drying conditionsTemperature: ..
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
ISO 180
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene
SV - 0157 ABS extrusion grade has been formulated to provide excellent mechanical properties, extrusion stability, vacuum formability and chemical resistance. It has low flow with high impact streng..
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific)
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched (ISO) 31.0 kJ/m²

@Temperature 0.000 °C
14.8 ft-lb/in²

@Temperature 32.0 °F
80*10*4mm, Cut; ISO 180/1A
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP
SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig..
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRILOY D20001 PPO
LNP* LUBRILOY* Z20001 is a compound based on PPO resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357 PBT+PC
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357M PBT+PC
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP C7410 PC+ABS (Asia Pacific)
LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP)
LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU
LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber.
Izod Impact, Notched (ISO) 31.0 kJ/m²

@Temperature 23.0 °C
14.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Verton OV00A PPS (Asia Pacific)
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
ISO 180/1A
Chi Mei Polylac® PA-709 ABS
Super impact
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
ISO 180/1A
Chi Mei Polylac® PA-709S ABS - Extrusion
Super Impact Extrusion
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
1A; ISO 180
Azoty Tarnow™ TARNOFORM 200 HI4 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRILOY Z20001 PPO
LNP* Lubriloy* Z20001 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.
Izod Impact, Notched (ISO) 31.0 kJ/m²

@Temperature 23.0 °C
14.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Verton OV00A PPS
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON PX00700 PA 6
LNP VERTON* PX00700 is a compound based on Nylon 6 resin containing proprietary fillers. Added feature of this grade is: Structural.
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 (Asia Pacific)
LNP* Verton* PX00700 is a compound based on Nylon 6 resin containing Long Glass Fiber.