Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 2.70 - 40.0 kJ/m² | 1.28 - 19.0 ft-lb/in² | Average value: 13.1 kJ/m² Grade Count:5 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Izod Impact, Notched (ISO) | >= 2.70 kJ/m² | >= 1.28 ft-lb/in² | ISO 180-1A |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Izod Impact, Notched (ISO) | 2.70 kJ/m² | 1.28 ft-lb/in² | ISO 180-1A |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Izod Impact, Notched (ISO) | 2.70 kJ/m² | 1.28 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
Izod Impact, Notched (ISO) | 2.70 - 6.00 kJ/m² | 1.28 - 2.86 ft-lb/in² | Average value: 4.53 kJ/m² Grade Count:12 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched (ISO) | 2.70 - 6.00 kJ/m² | 1.28 - 2.86 ft-lb/in² | Average value: 3.67 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched (ISO) | 2.70 - 54.0 kJ/m² | 1.28 - 25.7 ft-lb/in² | Average value: 19.0 kJ/m² Grade Count:11 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Izod Impact, Notched (ISO) | 2.70 kJ/m² | 1.28 ft-lb/in² | ISO 180 |
Polyram RamTal PM340S6 Polyacetal for Injection Molding, 30% Glass-Beads Filled 30% Glass-beads filled polyacetal for injection molding applications.Information provided by Polyram. |