Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 2.50 - 12.0 kJ/m² | 1.19 - 5.71 ft-lb/in² | Average value: 6.75 kJ/m² Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180/1A |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -40.0 °C |
1.19 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Phillips Sumika Marlex® CHN-200 Thermoplastic Polyolefin
(discontinued **) Thermoplastic Polyolefin, High Stiffness, Talc-FilledApplications: Automotive InteriorsConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.9-1.1%Drying conditionsTemperature: 80-100°CTim.. |
|||
Izod Impact, Notched (ISO) | 2.50 - 47.0 kJ/m² | 1.19 - 22.4 ft-lb/in² | Average value: 8.19 kJ/m² Grade Count:104 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 2.50 - 12.0 kJ/m² | 1.19 - 5.71 ft-lb/in² | Average value: 5.29 kJ/m² Grade Count:33 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched (ISO) | 2.50 - 95.0 kJ/m² | 1.19 - 45.2 ft-lb/in² | Average value: 13.0 kJ/m² Grade Count:240 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Notched (ISO) | 2.50 - 47.0 kJ/m² | 1.19 - 22.4 ft-lb/in² | Average value: 14.3 kJ/m² Grade Count:111 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | Sample Type A; ISO 180:2000 |
Global EPP PET SL PET + Solid Lubricant PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Izod Impact, Notched (ISO) | >= 2.50 kJ/m² | >= 1.19 ft-lb/in² | ISO 180-1A |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig.. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180/A |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® FPTC 60 - 60% Talc & Calcium Carbonate Reinforced Polypropylene Homopolymer Masterbatch 60% Talc+Calcium Reinforced PP HomopolymerApplications: Furniture & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GSF1849-N1 Nylon 66, 40% Glass Sphere/Fiber Reinforced Developmental productAll information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GSF25/15-66 22LH-N 40% Glass Sphere/Fiber Reinforced Nylon 66 Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180 |
Total PPH 11012 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed .. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180 |
Total PPM H350 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H350 is a homopolymer with a Melt Flow Index of 35 g/10 min recommended for the manufacture of medical packaging and medical devices, to the exclusion of implants.Polypropylene PPM.. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 BK010 is a 30% mineral reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 652 Polypropylene Homopolymer High temperature resistance, high gloss, very good surface appearanceInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180/1A |
A.D. Compound Adene NCTA Homopolymer 50% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180/1A |
A.D. Compound Adene NTWA Homopolymer 60% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene J 490 M40S Flame Retardant Polypropylene, 40% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 2.50 - 100000 kJ/m² | 1.19 - 47600 ft-lb/in² | Average value: 14.6 kJ/m² Grade Count:33 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 442 M30 Polypropylene Homopolymer High heat resistance, detergent stabilizedInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² | 1.19 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 218 S30 is used in all sectors of indu.. |
|||
Izod Impact, Notched (ISO) | 2.50 - 100000 kJ/m² | 1.19 - 47600 ft-lb/in² | Average value: 11.1 kJ/m² Grade Count:19 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Izod Impact, Notched (ISO) | 2.50 - 100000 kJ/m² | 1.19 - 47600 ft-lb/in² | Average value: 6.56 kJ/m² Grade Count:10 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |