Polymer Property : Izod Impact, Notched (ISO) = 0.950 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.99 kJ/m²
0.950 ft-lb/in²
ISO 180/A
ExxonMobil PP1014H1 Polypropylene Homopolymer
Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE..
Izod Impact, Notched (ISO) 1.99 kJ/m²
0.950 ft-lb/in²
ISO 180/1A
ExxonMobil PP1064L1 Polypropylene Homopolymer
Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other ..
Izod Impact, Notched (ISO) 1.99 kJ/m²
0.950 ft-lb/in²
ISO 180/1A
ExxonMobil PP1364E2 Polypropylene Homopolymer
Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc..