Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 0.700 - 7.00 kJ/m² @Temperature -40.0 - -30.0 °C |
0.333 - 3.33 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.58 kJ/m² Grade Count:12 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched (ISO) | 0.700 kJ/m² @Temperature 23.0 °C |
0.333 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |