Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 0.510 kJ/m² | 0.243 ft-lb/in² | ASTM D256 |
Reliance Industries PVAXX H60 The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie.. |