Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.00 - 80.0 kJ/m² | 3.81 - 38.1 ft-lb/in² | Average value: 31.8 kJ/m² Grade Count:15 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched (ISO) | 60.0 - 80.0 kJ/m² | 28.6 - 38.1 ft-lb/in² | Average value: 66.7 kJ/m² Grade Count:6 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 80.0 kJ/m² | 1.43 - 38.1 ft-lb/in² | Average value: 15.8 kJ/m² Grade Count:18 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |