Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.50 - 60.0 kJ/m² | 1.67 - 28.6 ft-lb/in² | Average value: 8.52 kJ/m² Grade Count:75 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 60.0 kJ/m² @Temperature -40.0 - 0.000 °C |
1.43 - 28.6 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 10.7 kJ/m² Grade Count:54 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 3.50 - 60.0 kJ/m² | 1.67 - 28.6 ft-lb/in² | Average value: 17.0 kJ/m² Grade Count:27 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 60.0 kJ/m² | 2.38 - 28.6 ft-lb/in² | Average value: 26.9 kJ/m² Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched (ISO) | 60.0 - 60.0 kJ/m² @Temperature -20.0 - -20.0 °C |
28.6 - 28.6 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 15.1 kJ/m² Grade Count:3 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 60.0 kJ/m² | 0.952 - 28.6 ft-lb/in² | Average value: 7.59 kJ/m² Grade Count:44 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |