Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C |
1.43 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.33 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Izod Impact, Notched (ISO) | 5.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C |
2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.00 kJ/m² Grade Count:1 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Izod Impact, Notched (ISO) | 4.00 - 5.00 kJ/m² @Temperature -40.0 - -40.0 °C |
1.90 - 2.38 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 4.33 kJ/m² Grade Count:3 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 5.00 kJ/m² | 1.43 - 2.38 ft-lb/in² | Average value: 4.22 kJ/m² Grade Count:9 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C |
2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.00 kJ/m² Grade Count:1 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 5.00 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 2.38 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.25 kJ/m² Grade Count:6 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched (ISO) | 4.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C |
1.90 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.50 kJ/m² Grade Count:2 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C |
2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.00 kJ/m² Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C |
2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.00 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |