Polymer Property : Izod Impact, Notched (ISO) = 21.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.00 - 21.0 kJ/m²

@Temperature -40.0 - -30.0 °C
1.43 - 9.99 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 7.14 kJ/m² Grade Count:22
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..