Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.50 - 17.0 kJ/m² @Temperature -40.0 - -20.0 °C |
1.67 - 8.09 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 8.86 kJ/m² Grade Count:31 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched (ISO) | 3.70 - 17.0 kJ/m² | 1.76 - 8.09 ft-lb/in² | Average value: 11.3 kJ/m² Grade Count:11 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched (ISO) | 10.0 - 17.0 kJ/m² | 4.76 - 8.09 ft-lb/in² | Average value: 14.5 kJ/m² Grade Count:4 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |