Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 12.0 - 15.0 kJ/m² | 5.71 - 7.14 ft-lb/in² | ASTM D256 |
Polikim EFALON® C-25 PTFE, 25% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Izod Impact, Notched (ISO) | 10.0 - 15.0 kJ/m² | 4.76 - 7.14 ft-lb/in² | Average value: 12.2 kJ/m² Grade Count:6 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Izod Impact, Notched (ISO) | 2.60 - 15.0 kJ/m² @Temperature -20.0 - -20.0 °C |
1.24 - 7.14 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 5.34 kJ/m² Grade Count:13 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Izod Impact, Notched (ISO) | 2.60 - 15.0 kJ/m² | 1.24 - 7.14 ft-lb/in² | Average value: 7.65 kJ/m² Grade Count:18 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Izod Impact, Notched (ISO) | 11.0 - 15.0 kJ/m² @Temperature -40.0 - -40.0 °C |
5.23 - 7.14 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 12.8 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Izod Impact, Notched (ISO) | 10.0 - 15.0 kJ/m² @Temperature -40.0 - -30.0 °C |
4.76 - 7.14 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 11.1 kJ/m² Grade Count:7 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched (ISO) | 4.00 - 15.0 kJ/m² @Temperature -40.0 - -40.0 °C |
1.90 - 7.14 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 9.83 kJ/m² Grade Count:8 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched (ISO) | 3.99 - 15.0 kJ/m² | 1.90 - 7.14 ft-lb/in² | Average value: 8.00 kJ/m² Grade Count:7 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 15.0 kJ/m² | 2.38 - 7.14 ft-lb/in² | Average value: 10.0 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 15.0 kJ/m² | 3.33 - 7.14 ft-lb/in² | Average value: 12.5 kJ/m² Grade Count:11 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 15.0 - 15.0 kJ/m² @Temperature -30.0 - -30.0 °C |
7.14 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 15.0 kJ/m² Grade Count:1 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |