Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CM4219 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180 |
PolyOne Nymax™ GF 1800 35 HS Natural Polyamide 612 (Nylon 612) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Colorcomp DX98735 PC LNP COLORCOMP* DX98735 is a compound based on Polycarbonate resin containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP LCL36 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL36 is a compound based on Polyetheretherketone containing Carbon Fiber , PTFE. Added features of this material include Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 180/1A |
SABIC Innovative Plastics SABIC PPCOMPOUND 5521 PP SABIC® PPcompound 5521 is a mineral filled, impact modified polypropylene TPO. This material combines good flow with exterior automotive weathering stability. The general purpose black color prod.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing, Flame Retardant... |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific) LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific) LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -40.0 °C |
4.28 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East) Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66 LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for .. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP RFP48SXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFP48SXS is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA6.12 (Europe-Africa-Middle East) LNP THERMOCOMP* IF006 is a compound based on nylon 6/12 resin containing glass fibre |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding... |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF33A099-HRBK Nylon 66, 33% Glass Fiber Reinforced, Hydrolysis Resistant All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180/1A |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 200 LS POM Injection molding grade based on Tarnoform 200 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² - NB | 4.28 ft-lb/in² - NB | Average value: 25.4 kJ/m² Grade Count:27 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl C2 V20 Nylon 66/6, 20% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |