Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 161 PC (Europe-Africa-Middle East) LEXAN 161 is a medium viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 164R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with b.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 263R PC (Europe-Africa-Middle East) LEXAN 263R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 920A PC (Europe-Africa-Middle East) LEXAN 920A is a medium viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 945AU PC (Europe-Africa-Middle East) Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 955 PC (Europe-Africa-Middle East) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 955AU PC (Europe-Africa-Middle East) Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 9945A PC (Europe-Africa-Middle East) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® AD143 PC (Europe-Africa-Middle East) LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9330P PC COPOLYMER (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD921A PC (Europe-Africa-Middle East) LEXAN FXD921A is a transparent/translucent, medium viscosity, flame retardent grade for light diffusion special effects. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East) Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP4R PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML104R PC (Europe-Africa-Middle East) LEXAN ML104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility inform.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® OQ3820 PC High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 925AU PC (Europe-Africa-Middle East) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 945A PC (Europe-Africa-Middle East) Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Asia Pacific) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC0703 PC (Asia Pacific) PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | ISO 180/1eA |
Lubrizol ESTALOC® 59200 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPS6R PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable... |