Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.86 kJ/m² | 3.74 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF25-66 XE-N 25% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |