Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.80 - 100 kJ/m² | 3.71 - 47.6 ft-lb/in² | Average value: 16.1 kJ/m² Grade Count:20 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Notched (ISO) | 7.80 - 29.6 kJ/m² | 3.71 - 14.1 ft-lb/in² | Average value: 17.1 kJ/m² Grade Count:7 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched (ISO) | 7.80 kJ/m² | 3.71 ft-lb/in² | ISO 180 |
LNP Thermocomp® LC-1006 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched (ISO) | 7.80 - 11.4 kJ/m² | 3.71 - 5.42 ft-lb/in² | Average value: 9.50 kJ/m² Grade Count:5 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 7.80 kJ/m² | 3.71 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient.. |
|||
Izod Impact, Notched (ISO) | 7.80 kJ/m² | 3.71 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hGC51 PPS / AE Polyphenylene Sulfide Injection molding, conductiveInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Izod Impact, Notched (ISO) | 7.80 kJ/m² | 3.71 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn.. |
|||
Izod Impact, Notched (ISO) | 7.80 kJ/m² | 3.71 ft-lb/in² | ISO 180/1A |
Cathay PA511 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Izod Impact, Notched (ISO) | 7.80 kJ/m² | 3.71 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of .. |
|||
Izod Impact, Notched (ISO) | 7.80 kJ/m² | 3.71 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers. |