Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.60 kJ/m² | 3.62 ft-lb/in² | ISO 180 |
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Izod Impact, Notched (ISO) | 7.60 kJ/m² | 3.62 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Izod Impact, Notched (ISO) | 7.60 kJ/m² | 3.62 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |