Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.10 - 79.0 kJ/m² | 3.38 - 37.6 ft-lb/in² | Average value: 18.9 kJ/m² Grade Count:57 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Izod Impact, Notched (ISO) | 7.10 kJ/m² | 3.38 ft-lb/in² | ISO 180-1A |
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 7.10 kJ/m² | 3.38 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 GF5 POM 26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Izod Impact, Notched (ISO) | 7.10 kJ/m² | 3.38 ft-lb/in² | ISO 180 |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |