Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.93 kJ/m² | 3.30 ft-lb/in² | ASTM D256 |
Nilit Polynil® P200 High Viscosity Nylon 66 Description: High viscosityApplication: Semi-finished and FilmInformation provided by NILIT. |
|||
Izod Impact, Notched (ISO) | 6.93 kJ/m² | 3.30 ft-lb/in² | ASTM D256 |
Nilit Polynil® P230 High Viscosity Nylon 66 Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various.. |
|||
Izod Impact, Notched (ISO) | 6.93 kJ/m² | 3.30 ft-lb/in² | ASTM D256 |
Nilit Polynil® P240 High Viscosity Nylon 66 Description: Polynil P240 is a high viscosity NYLON 66 (Viscosity number 290 cm³/gr) that was developed for rod and slab extrusion. It has a high melt stability and a low gel content.Key characteri.. |
|||
Izod Impact, Notched (ISO) | 6.93 kJ/m² | 3.30 ft-lb/in² | ASTM D256 |
Nilit Polynil® P240HSLV High Viscosity, Heat Stabilized Nylon 66 Description: Polynil P240 HSLV was developed for injection molding applications, where a combination of heat aging resistance, abrasion resistance and impact strength is needed, such as chain tensio.. |
|||
Izod Impact, Notched (ISO) | 6.93 kJ/m² | 3.30 ft-lb/in² | ISO 180/1A |
ExxonMobil HDPE HMA 025 High Density Polyethylene Resin Product Description: HMA 025 is a HDPE grade, characterized by excellent dimensional stability, impact strength and very high stiffness. Availability: Africa & Middle East, Asia Pacific and Europe A.. |
|||
Izod Impact, Notched (ISO) | 6.93 kJ/m² | 3.30 ft-lb/in² | ISO 180/1A |
ExxonMobil HDPE HMA 035 High Density Polyethylene Resin Product Description: HMA 035 is a UV stabilized HDPE grade, characterized by excellent dimensional stability, good impact strength and very high stiffness. Availability: Africa & Middle East, Asia .. |