Polymer Property : Izod Impact, Notched (ISO) = 56.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 56.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
26.6 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio..
Izod Impact, Notched (ISO) 56.0 kJ/m²

@Temperature -30.0 °C
26.6 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are..
Izod Impact, Notched (ISO) 56.0 kJ/m²
26.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
Izod Impact, Notched (ISO) 56.0 kJ/m²
26.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
Izod Impact, Notched (ISO) 56.0 kJ/m²
26.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer
Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) ..
Izod Impact, Notched (ISO) 56.0 kJ/m²
26.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Asia Pacific)
Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) ..
Izod Impact, Notched (ISO) 56.0 kJ/m²

@Temperature -30.0 °C
26.6 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific)
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color..
Izod Impact, Notched (ISO) 56.0 kJ/m²
26.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific)
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Izod Impact, Notched (ISO) 56.0 kJ/m²
26.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC
LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
Izod Impact, Notched (ISO) 56.0 kJ/m²

@Temperature 23.0 °C
26.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC
LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied..
Izod Impact, Notched (ISO) 56.0 kJ/m²

@Temperature -50.0 °C
26.6 ft-lb/in²

@Temperature -58.0 °F
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou..
Izod Impact, Notched (ISO) 56.0 - 56.0 kJ/m²

@Temperature -50.0 - -50.0 °C
26.6 - 26.6 ft-lb/in²

@Temperature -58.0 - -58.0 °F
Average value: 56.0 kJ/m² Grade Count:1
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade