Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 50.4 kJ/m²
24.0 ft-lb/in²
ISO 180/A
ExxonMobil Exxtral™ H1025W Performance Polyolefin
Product Description: A polyolefin injection molding compound designed with good flow, cold temperature impact resistance, low CLTE, weatherable mold-in-color and also suitable for painted automotive..
Izod Impact, Notched (ISO) 50.4 kJ/m²
24.0 ft-lb/in²
ISO 180/1A
ExxonMobil PP8013L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t..