Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 46.2 kJ/m² | 22.0 ft-lb/in² | ISO 180/A |
ExxonMobil Exxtral™ BMU130A Performance Polyolefin Product Description: Polyolefin injection molding compound with a good balance of stiffness, flow, and excellent processability for automotive bumper fascia and exterior trim applicationsAvailabilit.. |
|||
Izod Impact, Notched (ISO) | 46.2 kJ/m² | 22.0 ft-lb/in² | ISO 180/1A |
ExxonMobil LLDPE L L6101RQ Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness .. |
|||
Izod Impact, Notched (ISO) | 46.2 kJ/m² | 22.0 ft-lb/in² | ISO 180/1A |
ExxonMobil LLDPE LL 6101XR Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness .. |