Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.40 kJ/m²
2.09 ft-lb/in²
ISO 180
Polyram PlusTek PA700BL10 Nylon 6.6 for Injection Molding, UV Stabilized
UV Stabilized Nylon 6.6 for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 4.40 kJ/m²
2.09 ft-lb/in²
ISO 180
Polyram PlusTek RA702 Nylon 66 for Injection Molding, UV Stabilized
UV stabilized Nylon 66 for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 4.40 kJ/m²
2.09 ft-lb/in²
ASTM D256
Tipco Tipcolene® ISL 10 BX1 - 10% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow, Stiffness & Impact Strength
10% Mineral Reinforced, High Stiffness, High Impact PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., Indi..