Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS Cycoloy Medium Heat Plating Grade for Automotive |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | NB; ISO 180/1A |
Dow INSPIRE™ D7000 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ASTM D638 |
Iran Petrochemical (PCC) Moplen Z 30 G Polypropylene Moplen Z 30 G is a high flow homopolymer for injection molding and compounding applications. Moplen Z 30 G exhibits a high stiffness and an outstanding processability for shorter cycle times and eas.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ISO 180-1A |
Gromax BTE30-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -10.0 °C |
14.3 ft-lb/in² @Temperature 14.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON WV006 PBT (Europe-Africa-Middle East) LNP VERTON* WV006 is a compound based on Polybutylene Terephalate resin containing Long Glass. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ASTM D 256 |
Lubrizol Telene 1650 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ISO 180 |
Polyram Polytron P30N03 Polypropylene, 30% Long Glass Fibers A chemically coupled 30% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance chara.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® FR3040 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD4471 PC Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |