Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 0.000 °C |
9.04 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Faradex MS003XXC PP (Europe-Africa-Middle East) LNP* Faradex* MS003XXC is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.This data was supplied by SABIC-IP for.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP FARADEX MX10014 PP (Europe-Africa-Middle East) LNP* Faradex* Mx10014 is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® Rapide CLG 910B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific) LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC LNP* LUBRICOMP* DX94375H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 180/1A |
SYNTHOS Forsan® 449 Acrylonitrile Butadiene Styrene (ABS) High flow, high gloss, suitable for electroplating.Applications: General purpose, intricate and thin-walled productsHousehold appliances, vacuum cleaners, heels, toys, fan grilles, etc.Synthos was f.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO Test |
Styrolution Terluran® HH-106 ABS Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA 6/10 (Europe-Africa-Middle East) LNP* Thermocomp* QF00A is a compound based on Nylon 6/10 resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific) LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180 |
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST801AHS BK010 Nylon 66
(Unverified Data**) Super Toughened Heat Stabilized Polyamide 66 Zytel ST801AHS BK010 is a Super Tough high performance black polyamide 66 resin. It offers outstanding molding performance in injection molding applicati.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Staramide PF00AS PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AS is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-777B ABS - High Heat High Heat Impact |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 0.000 °C |
9.04 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |