Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® OQ1022 PC (Asia Pacific) Standard Flow OQ Resin |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP ZI001 PPE+PS LNP* LUBRICOMP ZI001 is a compound based on PPE+PS resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp DF0069E PC LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF008XXZ is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP UF009AS PPA (Europe-Africa-Middle East) LNP* Thermocomp* UF009AS is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV005SX0 PP (Europe-Africa-Middle East) LNP* VERTON* MV005SX0 is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RF008S PA 66 LNP* THERMOCOMP* RF008S is a compound based on Nylon 6/6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GFX1872-N1 (PTFE) Nylon 66, 33% Glass Reinforced, Lubricated All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ASTM D256 |
Total PSI 8350 (AS) High Impact Polystyrene Total Petrochemicals Polystyrene 8350 (AS) is a very high impact polystyrene for extrusion and injection molding. This grade has improved environmental stress crack resistance in comparison with st.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® SEB 300 M - 30% Chemically Coupled Glass Fibers & Mineral Polypropylene Homopolymer 30% Mineral + Glass Reinforced, PP Homopolymer for Automobile Engine PartsApplications: Automotive Engine PartsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® FR3005 BBS310 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecolen® HP10 GR30 NL HS PPCP, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO Test |
BASF Ultramid® 1000-2 NF2001 PA66 (Conditioned) Ultramid 1000-2 NF2001 is a general purpose PA6/6. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO Test |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 3146 |
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry) Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® XT1863-BK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |