Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.99 kJ/m² | 0.950 ft-lb/in² | ISO 180/A |
ExxonMobil PP1014H1 Polypropylene Homopolymer Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE.. |
|||
Izod Impact, Notched (ISO) | 1.99 kJ/m² | 0.950 ft-lb/in² | ISO 180/1A |
ExxonMobil PP1064L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Izod Impact, Notched (ISO) | 1.99 kJ/m² | 0.950 ft-lb/in² | ISO 180/1A |
ExxonMobil PP1364E2 Polypropylene Homopolymer Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc.. |