| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS
LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP FARADEX NS0031 PC+ABS (Asia Pacific)
Faradex NS0031 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel. Added features of this material include: EMI/RFI Shiel..
|
|||
| Izod Impact, Unnotched (ISO) |
39.0
kJ/m² @Temperature -30.0 °C |
18.6
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP FARADEX NS0031 PC+ABS (Asia Pacific)
Faradex NS0031 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel. Added features of this material include: EMI/RFI Shiel..
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC
LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant.
|
|||
| Izod Impact, Unnotched (ISO) |
39.0
-
47.0
kJ/m² @Temperature -30.0 - -30.0 °C |
18.6
-
22.4
ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 42.7 kJ/m² Grade Count:5 |
|
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | |
|
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12
LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer
LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer
LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66
LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12
LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA
LNP* LUBRICOMP* UCL36S is a compound based on Polyphthalamide resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Heat Stabilized, Electrically Con..
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA (Asia Pacific)
LNP* Lubricomp* UCL36S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond..
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | ISO 180 |
|
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining..
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP STAT-KON DE002ER PC
LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific)
LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP STAT-KON DE003Z PC
LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP PFW64 PA 6
LNP* THERMOCOMP* PFW64 is a compound based on Nylon 6 resin containing 20% Glass Fiber, 30% Wollastonite.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66
LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare.
|
|||
| Izod Impact, Unnotched (ISO) |
39.0
kJ/m² @Temperature 23.0 °C |
18.6
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermocomp RFZ349 PA 66 (Asia Pacific)
LNP* Thermocomp* RFZ349 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t..
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66
LNP THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% Milled Glass. Added features of this material include: Flame Retardant.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA
LNP THERMOCOMP* UX05504 is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA (Asia Pacific)
LNP* THERMOCOMP* UX05504 is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP WF006L PBT
LNP* THERMOCOMP* WF006L is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this material is: Low Extractible.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 (Asia Pacific)
LNP* THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | ISO 180 |
|
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific)
LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP WF002I PBT
LNP* THERMOTUF* WF006I is a compound based on PBT resin containing 10% Glass Fiber. Added feature of this grade is: High Impact.
|
|||
| Izod Impact, Unnotched (ISO) | 39.0 kJ/m² | 18.6 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC
LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated.
|
|||