Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 86.0 kJ/m² | 40.9 ft-lb/in² | d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 40H2.0 EF 900116 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 86.0 kJ/m² | 40.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 86.0 kJ/m² | 40.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXH PA 66 LNP* THERMOCOMP* RF008XXH is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 86.0 kJ/m² | 40.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Izod Impact, Unnotched (ISO) | 86.0 kJ/m² | 40.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 (Asia Pacific) LNP* Verton* PV007 is a compound based on Nylon 6 resin containing Long Glass Fiber. |