Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP PL002 PA 6
LNP* LUBRICOMP* PL002 is a compound based on Nylon 6 base resin containing 10% PTFE. Added feature of this grade is: Wear Resistant.
Izod Impact, Unnotched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66
LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE
LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber.
Izod Impact, Unnotched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC
LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding.
Izod Impact, Unnotched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific)
LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding.
Izod Impact, Unnotched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6
LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers.
Izod Impact, Unnotched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RX00327 PA 66
LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural.