Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Qualchem Danamid FGF-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180/1U |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Izod Impact, Unnotched (ISO) | 50.0 - 82.0 kJ/m² | 23.8 - 39.0 ft-lb/in² | Average value: 62.7 kJ/m² Grade Count:7 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 - 105 kJ/m² @Temperature -40.0 - -30.0 °C |
23.8 - 50.0 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 73.8 kJ/m² Grade Count:9 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 50.0 - 90.0 kJ/m² | 23.8 - 42.8 ft-lb/in² | Average value: 79.3 kJ/m² Grade Count:7 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFL25ES PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL25ES is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RN001 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RN001 is a compound based on Nylon 66 resin containing MOS2. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RN001XXC PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RN001XXC is a compound based on Nylon 66 resin containing MOS2. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON CX99000 PS (Europe-Africa-Middle East) LNP* STAT-KON* CX99000 is a compound based on Polystyrene containing Carbon Powder. Added features include : Electrically Conductive, Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East) LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RF007ESS PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF007ESS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* WF006 is a compound based on Polybutylene Terephalate resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180A |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® HR5330HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF003S PA66, 15% Glass Fiber Filled, Injection Molded Staramide RF003S is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G15 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-MFC-G0 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-MFC-G20 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
BLUESTAR 201G20 PBT, 20% Glass Filled Typical Applications: Energy saving lightingInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1U |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV008SXP PP (Europe-Africa-Middle East) LNP* Verton* MV008SXP is a compound based on Polypropylene resin containing Long Glass. Added features include: Chemically Coupled, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |