Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC LNP* LUBRICOMP* DFP36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² @Temperature 23.0 °C |
23.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | Type 1; ISO 180 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² @Temperature 23.0 °C |
23.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV006S PP LNP* VERTON* MV006S is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Structural. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV006S PP (Asia Pacific) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV006S PP (Europe-Africa-Middle East) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV006SU PP LNP VERTON* MV006SU is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV006SU PP (Asia Pacific) LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV006SU PP (Europe-Africa-Middle East) LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA6.10 LNP* LUBRICOMP* QCP36 is a compound based on Nylon 6/10 resin containing 15% PTFE/Silicone, 30% Carbon Fiber. Added features of this material include: Wear Resistant. Electrically Conductive |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | Type 1; ISO 180 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Izod Impact, Unnotched (ISO) | 49.0 kJ/m² | 23.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCP36 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conducti.. |